Products > STAINLESS SPRING WIRE

   


Comparisontable of stainless steel grades

China

Japan

USA

EU

GB

JIS

ASTM

EN

12Cr17Ni7

 

301

1.4310

12Cr18Ni9

SUS302

302

1.4325

0Cr18Ni9

SUS304

304

1.4301

07Cr19Ni10

 

304H

1.4948

022Cr98Ni10

SUS304L

304L

1.4307

06Cr19Ni10N

SUS304N1

304N

1.4315

06Cr25Ni20

SUS310S

310S

1.4845

06Cr17Ni12Mo2

SUS316

316

1.4401

022Cr17Ni12Mo

SUS316L

316L

1.4404

06Cr17Ni12Mo2N

SUS316N

316N

 

06Cr17Ni12Mo2Ti

SUS316Ti

316Ti

1.4571

06Cr18Ni11Ti

 

321

1.4541

07Cr17Ni7Al

SUS631J1

631

1.4568

10Cr17

SUS430

430

1.4016

12Cr13

SUS410

410

1.4006

Grade

MJIS     Chemical composition of stainless steel   (%)

C

Si

Mn

P

S

Ni

Cr

Mo

Other

SUS301

⩽0.15

⩽1.00

⩽2.00

⩽0.045

⩽0.030

6.00-8.00

16.00-18.00

 

 

SUS302

⩽0.15

⩽1.00

⩽2.00

⩽0.045

⩽0.030

8.00-10.00

17.00-19.00

 

 

SUS304

⩽0.08

⩽1.00

⩽2.00

⩽0.045

⩽0.030

8.00-10.50

18.00-20.00

 

 

SUS304L

⩽0.03

⩽1.00

⩽2.00

⩽0.045

⩽0.030

9.00-13.00

18.00-20.00

 

 

SUS304N1

⩽0.08

⩽1.00

⩽2.50

⩽0.045

⩽0.030

7.00-10.50

18.00-20.00

 

N:0.10-0.25

SUS316

⩽0.08

⩽1.00

⩽2.00

⩽0.045

⩽0.030

10.00-14.00

16.00-18.00

2.00-3.00

 

SUS316L

⩽0.03

⩽1.00

⩽2.00

⩽0.045

⩽0.030

12.00-15.00

16.00-18.00

2.00-3.00

 

SUS631J1

⩽0.09

⩽1.00

⩽1.00

⩽0.040

⩽0.030

7.00-8.50

16.00-18.00

 

AL:0.75-1.50

Properties

Steel type

Major component

Properties & Application

SUS301

17Cr-7Ni

High strength and good corrosion resistance after cold machining

SUS302

18Cr-8Ni-0.1Cu

Hight strength after cold machining,slightly worsestretching force than 301,exterior decaration materials of buildings

SUS304

18Cr-8Ni

Widely used as stainless steel,heat-resistant steel and food equipment

SUS316

18Cr-12Ni-2.5Mo

Better corrosion resistance than SUS304 in seawater and various organic acids

SUS316L

18Cr-12Ni-2.5Mo-N

A kind of low carbon steel as 316,but lower carbon content than 316,better intercrystailine corrosion resistance, an important corrorion-resistant material

SUS631

17Cr-7Ni-AL

A kind of stainless material with high strength and high temperature resistantce

SUS130M

10Cr18Mn9Ni5N

As a non-magnetic stainless steel with good corrosion resistance, it is widely used in electrical components and precision instruments

Accordingto JIS G 4314 standard

Wire diameter  mm

Tensile strength(N/mm2)

Series A

Series B

Series C

Series D

SUS302-WPA

SUS302-WPB

SUS631J1-WPC

SUS304-WPDS

SUS304-WPA

SUS304-WPB

SUS304Ni-WPA

SUS304-WPBS

SUS316-WPA

SUS304Ni-WPB

0.10-0.20

1650-1900

2150-2400

1950-2200

 

0.2-0.29

1600-1850

2050-2300

1930-2180

 

0.29-0.40

1700-2000

0.40-0.60

1950-2200

1850-2050

1650-1950

0.60-0.70

1530-1780

1850-2100

1800-2050

1550-1850

0.70-0.90

1550-1800

0.90-1.00

1550-1750

1.00-1.20

1450-1700

1750-2000

1700-1950

1470-1720

1.20-1.40

1420-1670

1.40-1.60

1400-1650

1650-1900

1600-1850

1370-1620

1.60-2.00

 

2.00-2.60

1320-1570

1550-1800

1500-1750

 

2.60-4.00

1230-1480

1450-1700

1400-1650

 

4.00-6.00

1100-1350

1350-1600

1300-1550